Figure 1. (A) DSC curve of Fe46.6Mo8.7Cr24.5B9.5C10Si0.6 amorphous alloy measured at a heating rate of 20 K·min-1. The inset is the XRD pattern of the Fe-Cr-Mo-Si-B-C. (B) S(Q) curves of Fe-Cr-Mo-Si-B-C annealed at different temperatures.
Figure 1. (A) DSC curve of Fe46.6Mo8.7Cr24.5B9.5C10Si0.6 amorphous alloy measured at a heating rate of 20 K·min-1. The inset is the XRD pattern of the Fe-Cr-Mo-Si-B-C. (B) S(Q) curves of Fe-Cr-Mo-Si-B-C annealed at different temperatures.