fig5
Figure 5. (A) CV profiles and (B) EIS spectra of the Zn//I2 batteries in pristine and ARS-containing ZnSO4 electrolytes; (C) Galvanostatic charge/discharge profiles of the ZnSO4 + ARS electrolyte and (D) rate performance of the ZnSO4 and ZnSO4 + ARS electrolyte over a current-density range of 0.1-4.0 A g-1. Extended cycling behavior of Zn//I2 batteries with and without ARS at (E) 0.2 A g-1 and (F) 1.0 A g-1. CV: Cyclic voltammetry; EIS: electrochemical impedance spectroscopy; ARS: alizarin red S.