fig6
Figure 6. (A) Discharge capacity and Coulombic efficiency at 30 °C and C/10 rate for a high-voltage (4.2 V) NMC622 cathode with Celgard (2325) separator and an LFP cathode (3.7 V) with an electrospun PAN separator; A Li metal was used for the anode (B) CV plot for the electrolyte at 1 mV/s scan rate obtained for a cell with LFP cathode and Li metal anode. LFP: Lithium iron phosphate; PAN: polyacrylonitrile; CV: cyclic voltammetry.