A potential hydrogen isotope storage material Zr<sub>2</sub>Fe: deep exploration on phase transition behaviors and disproportionation mechanism

Figure 1. XRD pattern (A) and SEM image correlating the EDS mapping micrographs (B) of as-cast Zr2Fe alloy; (C) Pressure vs. temperature during thermal vacuum degassing activation experiment; (D) XRD pattern of activated Zr2Fe alloy; (E) Hydriding kinetics of Zr2Fe after different activation conditions; (F) XRD pattern of Zr2FeH5 hydride. XRD: X-ray diffractometer; SEM: Scanning electron microscope; EDS: X-ray spectrometer; EDX: Energy dispersive X-ray spectroscopy.