fig3
Figure 3. TG-DSC of Li0L0 and Li0L4 powders treated with wet-dry routes. The purge gas is 80% N2 and 20% O2 monitoring the practical calcination and sintering under ambient air. The I~VII stages corresponded to the following reactions: I: 20~60 °C, CH3CHOHCH3 (l) → CH3CHOHCH3 (g); II: 80~230 °C, LiOH·H2O → LiOH·0.5H2O + H2O (g), H2O (Absorbed) → H2O (g), CO2